LUMINESCENCE AND AFTERGLOW PROPERTIES OF EU DOPED AND DY CO-DOPED SrAl4O7

Investor logo
Authors

MISEVIČIUS Martynas TÁBORSKÝ Petr PINKAS Jiří KAREIVA Aivaras

Year of publication 2014
Type Conference abstract
MU Faculty or unit

Central European Institute of Technology

Citation
Description SrAl4O7:Eu and SrAl4O7:Eu,Dy samples have been prepared using conventional solid state synthesis. Addition of boric acid improves phase purity and influences photoluminescence. Europium- doped samples show emission maxima at 485 nm and afterglow decay halftimes up to ~285 s. Co-doping with dysprosium shifts emission maxima to 467 nm and enhances afterglow decay lifetimes up to ~474 s.